射出小常識 The Tips of Injection

詳細介紹 Introduce



產生現象原因:


當水分、空氣未除盡時,即會產生此狀況;或模內有空氣或塑料局部產生過熱,亦會造成水痕;另外,水痕可能來自於其他因素,需詳加觀察,以判定結果。

Reason:


Water & Air not complete remove and cause the problem. It might be also case by the other reason so need to inspection in process.




產生水痕對策:


1. 塑膠料需預先乾燥,較不會產生此現象。
2. 背壓、螺桿轉速適當調整,成品較優質。
3. 螺桿鬆退距離不宜太長,完善成品。

Countermeasure:


1. The material dry in advance.
2. Adjust the Back pressure & speed of screw rotation.
3. The distance of screw suck back to long.
詳細介紹 Introduce



產生現象原因:


當水分、空氣未除盡時,即會產生此狀況;或模內有空氣或塑料局部產生過熱,亦會造成水痕;另外,水痕可能來自於其他因素,需詳加觀察,以判定結果。

Reason:


Water & Air not complete remove and cause the problem. It might be also case by the other reason so need to inspection in process.




產生水痕對策:


1. 塑膠料需預先乾燥,較不會產生此現象。
2. 背壓、螺桿轉速適當調整,成品較優質。
3. 螺桿鬆退距離不宜太長,完善成品。

Countermeasure:


1. The material dry in advance.
2. Adjust the Back pressure & speed of screw rotation.
3. The distance of screw suck back to long.